This report presents thermal stability testing of fifteen Tracerco water tracers exposed to 250C for 48 hours. Tracer concentrations were compared using HPLC, with samples grouped based on retention time. Three tracers, HTP-001, HTP-002, and HTP-005, retained over 90% of their original concentration and passed the test. All other tracers showed significant degradation.

Citation Formats

TY - DATA AB - This report presents thermal stability testing of fifteen Tracerco water tracers exposed to 250C for 48 hours. Tracer concentrations were compared using HPLC, with samples grouped based on retention time. Three tracers, HTP-001, HTP-002, and HTP-005, retained over 90% of their original concentration and passed the test. All other tracers showed significant degradation. AU - Leggett, Smith DB - Open Energy Data Initiative (OEDI) DP - Open EI | National Renewable Energy Laboratory DO - KW - geothermal KW - energy KW - water tracers KW - thermal stability KW - tracer test KW - HPLC KW - high-temperature testing KW - retention time KW - tracer degredation KW - NaCl KW - Parr reactor KW - chemical tracer KW - concentration retention KW - high-temperature performance KW - duplicate testing KW - stability screening KW - technical report LA - English DA - 2025/04/11 PY - 2025 PB - Texas Tech University T1 - Tracerco High Temperature Tracer Thermal Stability Testing - Report UR - https://data.openei.org/submissions/8391 ER -
Export Citation to RIS
Leggett, Smith. Tracerco High Temperature Tracer Thermal Stability Testing - Report. Texas Tech University, 11 April, 2025, GDR. https://gdr.openei.org/submissions/1729.
Leggett, S. (2025). Tracerco High Temperature Tracer Thermal Stability Testing - Report. [Data set]. GDR. Texas Tech University. https://gdr.openei.org/submissions/1729
Leggett, Smith. Tracerco High Temperature Tracer Thermal Stability Testing - Report. Texas Tech University, April, 11, 2025. Distributed by GDR. https://gdr.openei.org/submissions/1729
@misc{OEDI_Dataset_8391, title = {Tracerco High Temperature Tracer Thermal Stability Testing - Report}, author = {Leggett, Smith}, abstractNote = {This report presents thermal stability testing of fifteen Tracerco water tracers exposed to 250C for 48 hours. Tracer concentrations were compared using HPLC, with samples grouped based on retention time. Three tracers, HTP-001, HTP-002, and HTP-005, retained over 90\% of their original concentration and passed the test. All other tracers showed significant degradation.}, url = {https://gdr.openei.org/submissions/1729}, year = {2025}, howpublished = {GDR, Texas Tech University, https://gdr.openei.org/submissions/1729}, note = {Accessed: 2025-05-09} }

Details

Data from Apr 11, 2025

Last updated Apr 17, 2025

Submitted Apr 11, 2025

Organization

Texas Tech University

Contact

Smith Leggett

Authors

Smith Leggett

Texas Tech University

Research Areas

DOE Project Details

Project Name Utah FORGE

Project Lead Lauren Boyd

Project Number EE0007080

Share

Submission Downloads